  • Cold Spray Zinc Anticorrosive Coating for High Voltage Wire Tower at -60º C to 300º C Temperature
  • Cold Spray Zinc Anticorrosive Coating for High Voltage Wire Tower at -60º C to 300º C Temperature
  • Cold Spray Zinc Anticorrosive Coating for High Voltage Wire Tower at -60º C to 300º C Temperature
  • Cold Spray Zinc Anticorrosive Coating for High Voltage Wire Tower at -60º C to 300º C Temperature
  • Cold Spray Zinc Anticorrosive Coating for High Voltage Wire Tower at -60º C to 300º C Temperature
  • Cold Spray Zinc Anticorrosive Coating for High Voltage Wire Tower at -60º C to 300º C Temperature
Color: Grey
Appearance: Liquid
Main Raw Material: Zinc Powder/Special Purpose Resin
Method: Brush/Roll/Spray
Level: Primer
Drying Method: Air Drying